Mechanical Properties Metric English Comments
Izod Impact, Unnotched 21.6 J/cm
40.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific)
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 21.6 J/cm
40.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Xenoy® X5500EX PBT+PC (Asia Pacific)
Non-FR, non-UV PC/PBT blend for film extrusion application
Izod Impact, Unnotched 21.6 J/cm
40.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC
LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Izod Impact, Unnotched 21.6 J/cm
40.5 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific)
Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys..