Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.62 J/cm | 4.90 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® M-40 40% Mica-Reinforced Polypropylene Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l.. |
|||
Izod Impact, Unnotched | 2.62 J/cm | 4.91 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 431 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 2.62 J/cm | 4.91 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 686 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |