Plastics Group Polifil® M-40 40% Mica-Reinforced Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Mica Filler
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® M-40 40% Mica-Reinforced Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in large area broad span applications where high modulus values are required and retained. Standard processing techniques are applicable.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Filler Content 40 %
40 %
ASTM D2584
Linear Mold Shrinkage 0.0080 cm/cm

@Thickness 1.59 mm
0.0080 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 8.0 - 12 g/10 min
8.0 - 12 g/10 min
230/2.16; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength at Break 30.8 MPa
4460 psi
ASTM D638
Flexural Modulus 5.17 GPa
750 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.470 J/cm
0.880 ft-lb/in
At 73°F; ASTM D256
Izod Impact, Unnotched 2.62 J/cm
4.90 ft-lb/in
At 73°F; ASTM D256
Gardner Impact 0.655 J
0.483 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
260 °F
ASTM D648