Izod Impact, Unnotched 2.47 J/cm
4.63 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT
LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity.