Polymer Property : Izod Impact, Unnotched = 2.20 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
4.12 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
PolyOne Maxxam™ PPC-40T Nat Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Izod Impact, Unnotched 2.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
4.12 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
PolyOne Maxxam™ PPH-10G Nat Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Izod Impact, Unnotched 2.20 J/cm
4.12 ft-lb/in
ASTM D256
Ineos Nova Zylar® 533 Clear Impact Modified UV Stabilized Acrylic Copolymer  (discontinued **)
Features: High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationExcellent indoor light stabilityHigh elongation and ductilityApplications: Appliance..
Izod Impact, Unnotched 2.20 J/cm
4.12 ft-lb/in
ASTM D256
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not ..
Izod Impact, Unnotched 2.20 J/cm
4.12 ft-lb/in
ASTM D256
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma..
Izod Impact, Unnotched 2.20 J/cm
4.12 ft-lb/in
ASTM D256
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a..
Izod Impact, Unnotched 2.20 J/cm
4.12 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6
LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity.