Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.189 J/cm | 4.101 ft-lb/in | ASTM D256 |
Stratasys® ABSi Stratasys is the only company that gives engineers the ability to manufacture real ABSi industrial thermoplastic parts direct from digital files. ABSi parts can be used from conceptual prototyping t.. |