Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 17.78 J/cm | 33.31 ft-lb/in | ASTM D4812 |
PlastiComp Complet® LGF60-PA66 MT 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |