Mechanical Properties Metric English Comments
Izod Impact, Unnotched 17.67 J/cm
33.10 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC
LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible.
Izod Impact, Unnotched 17.67 J/cm
33.10 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific)
LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
Copyright © lookpolymers.com All Rights Reserved