Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 17.4 J/cm | 32.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX91077 PC LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified. |