Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.71 J/cm | 16.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Izod Impact, Unnotched | 8.70 J/cm | 16.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
Izod Impact, Unnotched | 8.70 J/cm @Temperature 23.0 °C |
16.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp SX93441D PA6.12 LNP* Lubricomp* SX93441D is a compound based on Nylon 6/12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated.This data was supplied by SABIC-IP for the Ameri.. |
|||
Izod Impact, Unnotched | 8.70 J/cm | 16.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Unnotched | 8.72 J/cm @Temperature 23.0 °C |
16.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK LNP THERMOCOMP* LF004 is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 8.70 J/cm | 16.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA (Asia Pacific) LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 8.70 J/cm | 16.3 ft-lb/in | ASTM Test |
BASF Petra® 140 BK-112 45% Glass Filled PET Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa.. |
|||
Izod Impact, Unnotched | 8.70 J/cm @Thickness 3.18 mm |
16.3 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® UF-1008 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |