Polymer Property : Izod Impact, Unnotched = 15.2 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 8.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.2 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
PolyOne Maxxam™ PPC-20T Nat Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Izod Impact, Unnotched 8.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.2 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
PolyOne Trilliant™ HC X HC5200-0025 RS Natural Polypropylene Copolymer (PP Copolymer)
Information provided by PolyOne
Izod Impact, Unnotched 8.11 J/cm

@Temperature 23.0 °C
15.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp DFP22 PC
LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer..
Izod Impact, Unnotched 8.11 J/cm
15.2 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK
LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber.
Izod Impact, Unnotched 8.11 J/cm
15.2 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK (Asia Pacific)
LNP* Thermocomp* LF008 is a compound based on Polyetheretherketone resin containing Glass Fiber.