Polymer Property : Izod Impact, Unnotched = 14.41 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 14.41 J/cm
27.00 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Izod Impact, Unnotched 14.41 J/cm
27.00 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Izod Impact, Unnotched 14.41 J/cm
27.00 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Izod Impact, Unnotched 14.41 J/cm
27.00 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12
LNP* THERMOCOMP* SF008 is a compound based on Nylon 12 resin containing 40% Glass Fiber.
Izod Impact, Unnotched 14.41 J/cm
27.00 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON PV007 PA 6
LNP* VERTON* PV007 is a compound based on Nylon 6 resin containing 35% Long Glass Fiber. Added feature of this grade is: Structural.
Izod Impact, Unnotched 14.41 J/cm
27.00 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12 (Asia Pacific)
LNP* Thermocomp* SF008 is a compound based on Nylon 12 resin containing Glass Fiber.
Izod Impact, Unnotched 14.41 J/cm
27.00 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON PV007 PA 6 (Asia Pacific)
LNP* Verton* PV007 is a compound based on Nylon 6 resin containing Long Glass Fiber.