SABIC Innovative Plastics LNP VERTON PV007 PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON PV007 PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* PV007 is a compound based on Nylon 6 resin containing 35% Long Glass Fiber. Added feature of this grade is: Structural.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
1.40 g/cc
0.0506 lb/in³
ISO 1183
Moisture Absorption 1.30 %
1.30 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0049 cm/cm

@Time 86400 sec
0.0049 in/in

@Time 24.0 hour
ISO 294
0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 190 MPa
27600 psi
ASTM D638
Tensile Strength, Yield 190 MPa
27600 psi
ASTM D638
Elongation at Break 2.7 %
2.7 %
ASTM D638
Elongation at Yield 2.7 %
2.7 %
ASTM D638
Tensile Modulus 9.65 GPa
1400 ksi
50 mm/min; ASTM D638
Flexural Strength 296 MPa
42900 psi
ASTM D790
297 MPa
43100 psi
ISO 178
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
9.00 GPa
1310 ksi
ISO 178
Izod Impact, Notched 2.13 J/cm
3.99 ft-lb/in
ASTM D256
Izod Impact, Unnotched 14.41 J/cm
27.00 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 86.0 kJ/m²
40.9 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 7.00 J
5.16 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
212 °C

@Thickness 3.20 mm
414 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 209 °C
408 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
207 °C

@Thickness 3.20 mm
405 °F

@Thickness 0.126 in
unannealed; ASTM D648