Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 14.4 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2550® AM CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas 2550® AM CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generati..
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2550® CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas 2550® CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation ..
Izod Impact, Unnotched 7.70 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
14.4 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PP 1373
PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Izod Impact, Unnotched 7.69 J/cm
14.4 ft-lb/in
ASTM D-4812
PlastiComp Complet® LCF30-PA12 Nylon 12, 30% Long Carbon Fiber Content
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 30% long carbon fiber reinforcementInformation provided by PlastiComp, I..
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East)
VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings.
Izod Impact, Unnotched 7.70 J/cm

@Temperature -30.0 °C
14.4 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East)
VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings.
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® IQ420 PBT
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Izod Impact, Unnotched 7.68 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK
LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive.
Izod Impact, Unnotched 7.71 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP LX03447 PEEK
LNP* THERMOCOMP* LX03447 is a compound based on Polyetheretherketone containing Proprietary Filler(s).
Izod Impact, Unnotched 7.68 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON MV006S PP
LNP* VERTON* MV006S is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Structural.
Izod Impact, Unnotched 7.68 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON MV006S PP (Asia Pacific)
LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Izod Impact, Unnotched 7.68 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON MV006S PP (Europe-Africa-Middle East)
LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Izod Impact, Unnotched 7.68 J/cm

@Temperature -30.0 °C
14.4 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA
High flow PPO+PA. Power distribution box applications.
Izod Impact, Unnotched 7.68 J/cm

@Temperature -30.0 °C
14.4 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific)
High flow PPO+PA. Power distribution box applications.
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® IQ420HP PBT
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comshield® 120 Copolymer Polypropylene, Electrically Conductive - Carbon Black Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 7.70 J/cm
14.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON MV006BS PP
LNP* VERTON* MV006BS is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this grade include: Heat Stabilized, Burst Pressure, Structural, Chemically Coupl..
Copyright © lookpolymers.com All Rights Reserved