Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 13.88 J/cm | 26.00 ft-lb/in | ASTM D4812 |
PlastiComp Complet® LGF30-PA66 MT 30% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Unnotched | 13.88 J/cm | 26.00 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Izod Impact, Unnotched | 13.88 J/cm | 26.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DL0039E PC LNP* Lubricomp* DL0039E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant, Easy Molding. |
|||
Izod Impact, Unnotched | 13.88 J/cm | 26.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DL0039E PC (Asia Pacific) LNP* Lubricomp* DL0039E is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant, Easy Molding. |
|||
Izod Impact, Unnotched | 13.88 J/cm | 26.00 ft-lb/in | ASTM Test |
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Dry) Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil.. |