PlastiComp Complet® LGF30-PA66 MT 30% Long Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LGF30-PA66 MT 30% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 155 MPa
22500 psi
ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D638
Tensile Modulus 9.31 GPa
1350 ksi
ASTM D638
Flexural Strength 269 MPa
39000 psi
ASTM D790
Flexural Modulus 8.28 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 13.88 J/cm
26.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
469 °F
ASTM D648