Polymer Property : Izod Impact, Unnotched = 1.54 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.820 J/cm
1.54 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON ME006 PP
LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.