Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.27 J/cm | 2.38 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP KONDUIT PX11422 PA 6 LNP* KONDUIT* is a compound based on Nylon 6 resin containing thermally conductive fillers. Added feature of this material is Electrically Conductive. |
|||
Izod Impact, Unnotched | 1.27 J/cm @Thickness 3.17 mm |
2.39 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tribit® 1503S Polybutylene Terephthalate Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang |