Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP KONDUIT PX11422 PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Konduit
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP KONDUIT PX11422 PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* KONDUIT* is a compound based on Nylon 6 resin containing thermally conductive fillers. Added feature of this material is Electrically Conductive.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 53.0 MPa
7690 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.0 %
1.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 9.69 GPa
1410 ksi
5 mm/min; ASTM D638
Flexural Strength 82.0 MPa
11900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.21 GPa
1340 ksi
ASTM D790
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.27 J/cm
2.38 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Thermal Conductivity 2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 174 °C

@Thickness 3.20 mm
345 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 10000 ohm
10000 ohm
ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved