Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.12 J/cm

@Thickness 3.17 mm
2.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PA6GF33BK Nylon 6, 33% Glass Fiber Filled
Information provided by Niche Polymer
Izod Impact, Unnotched 1.12 J/cm

@Thickness 3.17 mm
2.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PA6GF33N Nylon 6, 33% Glass Fiber Filled
Information provided by Niche Polymer
Izod Impact, Unnotched 1.12 J/cm

@Thickness 3.17 mm
2.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PPHG40BK Homopolymer PP, 40% Glass Fiber Filled
Information provided by Niche Polymer
Izod Impact, Unnotched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, 50% RH
Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by Gehri..