Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.883 J/cm
1.65 ft-lb/in
ASTM D256
Hyosung Topilene J340F PP
J340F Film Grade Impact CopolymerApplications: Retort CPPCharacteristics:ProcessabilityHigh impactInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.883 J/cm
1.65 ft-lb/in
ASTM D256
Hyosung Topilene J351F PP
J351F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.883 J/cm

@Thickness 3.17 mm
1.65 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A..
Izod Impact, Unnotched 0.883 J/cm

@Thickness 3.17 mm
1.65 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Tripet® 2500G30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati..
Izod Impact, Unnotched 0.883 J/cm

@Thickness 3.17 mm
1.65 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Tripet® 2550GN30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati..
Izod Impact, Unnotched 0.883 - 9.60 J/cm
1.65 - 18.0 ft-lb/in
Average value: 5.64 J/cm Grade Count:10
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..