J351F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.4 MPa
4270 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
Izod Impact, Unnotched 0.883 J/cm
1.65 ft-lb/in
ASTM D256
0.392 J/cm

@Temperature -10.0 °C
0.735 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 161 °C
322 °F
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648