Polymer Property : Izod Impact, Unnotched = 0.785 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.785 J/cm
1.47 ft-lb/in
ASTM D256
Hyosung Topilene HJ640 PP
HJ640 High Isostatic PP Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporatio..
Izod Impact, Unnotched 0.785 J/cm
1.47 ft-lb/in
ASTM D256
Hyosung Topilene J440F PP
J440F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.785 J/cm
1.47 ft-lb/in
ASTM D256
Hyosung Topilene J740 PP
J740 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporation..
Izod Impact, Unnotched 0.785 J/cm
1.47 ft-lb/in
ASTM D256
Hyosung Topilene R401 PP
R401 Extrusion Random CopolymerApplications:Extrusion blow moldingStationary sheetCharacteristics:TransparencyStiffnessInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.785 J/cm
1.47 ft-lb/in
ASTM D256
Hyosung Topilene J742S PP
J742S Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corpora..
Izod Impact, Unnotched 0.785 J/cm

@Thickness 3.17 mm
1.47 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samyang Trirex® 3025GRU10 Polycarbonate, 10% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..