Polymer Property : Izod Impact, Unnotched = 0.643 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.343 J/cm

@Temperature -10.0 °C
0.643 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Hyosung Topilene HJ740 PP
HJ740 High Isostatic PP Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporatio..
Izod Impact, Unnotched 0.343 J/cm

@Temperature -10.0 °C
0.643 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Hyosung Topilene J440F PP
J440F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.343 J/cm
0.643 ft-lb/in
ASTM D256
Hyosung Topilene J801R PP
J801R Injection Special Purpose GradeApplications: Electric home applianceCharacteristics:High stiffnessLong-term heat resistanceInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.343 J/cm

@Temperature -10.0 °C
0.643 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Hyosung Topilene J945 PP
J945 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.343 J/cm
0.643 ft-lb/in
ASTM D256
Hyosung Topilene J801 PP
J801 Injection Special Purpose GradeApplications:Disposable syringeTransparent productCharacteristics:TransparencyHigh stiffnessInformation provided by Hyosung Corporation