Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.278 J/cm

@Temperature -40.0 °C
0.520 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech PETG 3D Lenticular 3-D Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
Izod Impact, Unnotched 0.278 J/cm

@Temperature -40.0 °C
0.520 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech APET SP4110 Copolyester Sheet
Description: Copolyester SheetInformation provided by Spartech.