Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.216 J/cm | 0.404 ft-lb/in | ASTM D256 |
Hyosung Topilene S905 PP S905 Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation |