Polymer Property : Izod Impact, Unnotched = 0.216 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.216 J/cm
0.404 ft-lb/in
ASTM D256
Hyosung Topilene S905 PP
S905 Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation