Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 83.0 MPa @Temperature 593 °C, Time 3.60e+7 sec |
12000 psi @Temperature 1100 °F, Time 10000 hour |
1% creep |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Creep Strength | 83.0 MPa @Temperature 593 °C, Time 3.60e+7 sec |
12000 psi @Temperature 1100 °F, Time 10000 hour |
1% creep |
ATI Allegheny Ludlum 309H Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Creep Strength | 83.0 MPa @Temperature 593 °C, Time 3.60e+7 sec |
12000 psi @Temperature 1100 °F, Time 10000 hour |
1% creep |
ATI Allegheny Ludlum 309S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Creep Strength | 83.0 MPa @Temperature 593 °C, Time 3.60e+7 sec |
12000 psi @Temperature 1100 °F, Time 10000 hour |
1% creep |
ATI Allegheny Ludlum 309Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Creep Strength | 82.7 MPa @Temperature 204 °C, Time 1.98e+6 sec |
12000 psi @Temperature 400 °F, Time 550 hour |
0.1% creep strain |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |