Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 5.00 MPa | 725 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH |