Polymer Property : Creep Strength = 5.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Creep Strength 5.00 MPa
725 psi
2% elongation, 1000 h; DIN 53444
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene
Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH