Creep Strength 22.0 MPa
3190 psi
stress leading to 1% elongation; dry; ISO 899-1
Murtfeldt Murylon® HT Nylon 46
The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir..
Creep Strength 22.0 MPa
3190 psi
2% elongation, 1000 h; DIN 53444
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene
Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH
Creep Strength 22.0 MPa
3190 psi
2% elongation, 1000 h; DIN 53444
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Dry
Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH