Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 22.0 MPa | 3190 psi | stress leading to 1% elongation; dry; ISO 899-1 |
Murtfeldt Murylon® HT Nylon 46 The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir.. |
|||
Creep Strength | 22.0 MPa | 3190 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | 22.0 MPa | 3190 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Dry Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH |