Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 210 MPa @Temperature 600 °C, Time 3.60e+6 sec |
30500 psi @Temperature 1110 °F, Time 1000 hour |
|
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |