Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 0.0500 MPa @Temperature 150 °C, Time 57600 sec |
7.25 psi @Temperature 302 °F, Time 16.0 hour |
DIN 28090-2 |
Guarniflon SC 1200 Polytetrafluoroethylene Seal SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blen.. |
|||
Creep Strength | 0.0500 MPa @Temperature 150 °C, Time 57600 sec |
7.25 psi @Temperature 302 °F, Time 16.0 hour |
DIN 28090-2 |
Guarniflon SC 1600 Polytetrafluoroethylene Seal SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blen.. |