Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Guarniflon SC 1600 Polytetrafluoroethylene Seal

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Guarniflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Guarniflon SC 1600 Polytetrafluoroethylene Seal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blends are found in the areas of environmental improvement (they are asbestos free) and overall cost saving. Main applications in the chemical, petrochemical, pharmaceutical, food, paper industries, etc.Complies with FDA specifications.Information provided by Guarniflon®
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Creep Strength 0.0700 MPa

@Temperature 23.0 °C
10.2 psi

@Temperature 73.4 °F
DIN 28090-2
0.0500 MPa

@Temperature 150 °C,
Time 57600 sec
7.25 psi

@Temperature 302 °F,
Time 16.0 hour
DIN 28090-2
Compressive Modulus 0.00500 GPa

@Temperature 23.0 °C
0.725 ksi

@Temperature 73.4 °F
DIN 28090-2
0.00640 GPa

@Temperature 150 °C,
Time 57600 sec
0.928 ksi

@Temperature 302 °F,
Time 16.0 hour
DIN 28090-2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Chemical Properties Metric English Comments
Critical Pressure 80.0 bar
60000 torr
max
Descriptive Properties Value Comments
Color Light Blue
Compression Creep, MPa 14
150°C, 30 N/mm³
Leakage with Nitrogen, cm³/min 0.02
DIN 3535
Leakage, mg/s*m <.01
DIN 28090-2
max P x T , bar °C 11000
Recovery, mm 0.07
DIN 28090-2