Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 7.00 MPa @Strain 3.50 % |
1020 psi @Strain 3.50 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Yield Strength | 7.00 MPa @Strain 3.50 % |
1020 psi @Strain 3.50 % |
Conditioned; ISO 178 |
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66
(discontinued **) PA 6/66 |