Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 40.0 MPa @Strain 3.50 % |
5800 psi @Strain 3.50 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding PA 66, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Flexural Yield Strength | 40.0 MPa @Strain 3.50 % |
5800 psi @Strain 3.50 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66 PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS. |
|||
Flexural Yield Strength | 40.0 MPa @Strain 3.50 % |
5800 psi @Strain 3.50 % |
Conditioned; ISO 178 |
Lanxess Durethan® A 30 H3.0 000000 Nylon 66 PA 66, non reinforced, injection molding, heat-ageing stabilized |
|||
Flexural Yield Strength | 40.0 MPa @Strain 3.50 % |
5800 psi @Strain 3.50 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |