Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 175 MPa @Strain 3.50 % |
25400 psi @Strain 3.50 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Flexural Yield Strength | 175 MPa @Strain 3.50 % |
25400 psi @Strain 3.50 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Yield Strength | 175 MPa @Strain 3.50 % |
25400 psi @Strain 3.50 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |