Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 113.8 MPa @Temperature -40.0 °C |
16510 psi @Temperature -40.0 °F |
ASTM-D790 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |