Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 110 MPa @Strain 3.50 % |
16000 psi @Strain 3.50 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S H3.0 000000 Nylon 66, Injection Molding PA 66, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Flexural Yield Strength | 110 MPa @Temperature 24.0 °C |
16000 psi @Temperature 75.2 °F |
Long Beam, Dry |
Hexcel® HexPly® F522 Epoxy Resin, K285 Kevlar® Fabric Hexcel designation: K285-38"-F522; Kev. 49 1140Information provided by HexCel |