Mechanical Properties Metric English Comments
Charpy Impact Unnotched >= 21.0 J/cm²
>= 99.9 ft-lb/in²
ISO 11542/2
Polikim ULPOLEN® 1000 UHMWPE Standard
Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia..
Charpy Impact Unnotched 21.0 - 26.0 J/cm²

@Temperature -30.0 - -30.0 °C
99.9 - 124 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 22.8 J/cm² Grade Count:4
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Charpy Impact Unnotched 21.0 J/cm²
99.9 ft-lb/in²
Ineos ABS Lustran® E401
Very high surface resistance, high surface gloss.,Property data per ISO test methods.
Charpy Impact Unnotched 21.0 J/cm²
99.9 ft-lb/in²
ISO 179
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.