Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.80 - 2.10 J/cm²
8.57 - 9.99 ft-lb/in²
ISO 11542-2
Okulen® 1000 PE-UHMW, Colored
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal ..
Charpy Impact Unnotched 0.570 - 2.10 J/cm²
2.71 - 9.99 ft-lb/in²
Average value: 1.12 J/cm² Grade Count:17
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Charpy Impact Unnotched 1.596 - 2.10 J/cm²

@Temperature -30.0 - 0.000 °C
7.596 - 9.99 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 1.85 J/cm² Grade Count:1
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..