Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.596 - 2.10 J/cm² @Temperature -30.0 - 0.000 °C |
7.596 - 9.99 ft-lb/in² @Temperature -22.0 - 32.0 °F |
Average value: 1.85 J/cm² Grade Count:1 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |