Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.60 J/cm² | 40.9 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Charpy Impact Unnotched | 8.60 - 11.5 J/cm² | 40.9 - 54.7 ft-lb/in² | Average value: 10.1 J/cm² Grade Count:12 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Charpy Impact Unnotched | 8.60 J/cm² @Temperature 23.0 °C |
40.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax BFG45-DN00N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 8.60 J/cm² | 40.9 ft-lb/in² | 23; ISO 179/1eU |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Charpy Impact Unnotched | 8.60 J/cm² | 40.9 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Charpy Impact Unnotched | 8.60 J/cm² | 40.9 ft-lb/in² | ISO Data, Low Temp |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact Unnotched | 8.60 J/cm² | 40.9 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact Unnotched | 8.60 J/cm² @Temperature 30.0 °C |
40.9 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-60/4 W PA666-GF60 Product description: Grilon TSG-60/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact Unnotched | 8.60 J/cm² @Temperature 23.0 °C |
40.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Conditioned, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact Unnotched | 8.60 J/cm² @Temperature 23.0 °C |
40.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 8.60 J/cm² | 40.9 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |