Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 16.5 J/cm² @Temperature 23.0 °C |
78.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® DP BC 310 EF 000000 Nylon 6 PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow) |