Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.33 J/cm² @Temperature -30.0 °C |
34.9 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp.. |