Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.06 J/cm² @Temperature -30.0 °C |
33.6 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi.. |