Mechanical Properties Metric English Comments
Charpy Impact Unnotched 7.06 J/cm²

@Temperature -30.0 °C
33.6 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi..