Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.428 J/cm² | 25.83 ft-lb/in² | ISO 179-1:2007 |
CRP Technology Windform® GT Polyamide Glass Composite Processed by selective laser sintering (SLS). Windform® GT is a deep and dark black composite material based on polyamide fiber glass. After hand finishing, the color becomes shining and brighter... |