Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.428 J/cm²
25.83 ft-lb/in²
ISO 179-1:2007
CRP Technology Windform® GT Polyamide Glass Composite
Processed by selective laser sintering (SLS). Windform® GT is a deep and dark black composite material based on polyamide fiber glass. After hand finishing, the color becomes shining and brighter...